High-performance monoclinic zirconia

This product is produced using proprietary technology from Zhenzhong Company. It exhibits a unique coral-like structure at the microscopic level. Compared to ordinary fused zirconia, this product has advantages such as high purity, high activity, large specific surface area, and low sintering temperature. In the field of ceramic pigments, the large specific surface area is more suitable for the use of high-end zirconium-based pigments. In the field of friction braking, the unique coral branch structure significantly enhances the bonding and strength between polymer resins and zirconia particles. In the high-end refractory materials sector, high-performance monoclinic zirconia powder can greatly improve the sintering density of products, enhance thermal shock resistance, and reduce sintering temperature.

Telephone:

Key words:

High-performance monoclinic zirconia

Classification:

  • Product Description
  • Chemical Composition (%)

    Code

    Chemical Composition (%)

    ZrO2+HfO2

    SiO2

    Al2O3

    Fe2O3

    TiO2

    Z-10

    ≥98.5

    ≤0.50

    ≤0.10

    ≤0.04

    ≤0.10

    Z-15

    ≥99.2

    ≤0.30

    ≤0.10

    ≤0.04

    ≤0.10

    Z-12

    ≥99.2

    ≤0.30

    ≤0.10

    ≤0.04

    ≤0.10

    Physical Performance Parameters

    Appearance

    BET

    White Powder

    3.0-8.0 m²/g

    Product Particle Size

    Code

    Z-10

    Z-15

    Z-12

    Particle Size (μm)

    3

    1.5

    0.8

    Main Applications

    High-quality ceramic pigments (high-temperature praseodymium yellow and zirconium iron red), high-quality refractory materials, PZT and dielectric materials, grinding materials, thermal barrier coatings, friction braking, and advanced technical ceramics, etc.

     


Previous Fused monoclinic zirconia

Next Fused calcia stabilized zirconia


Product inquiry

We will contact you within one working day. Please pay attention to your email.

All
  • All
  • Product Management
  • News