Silica fume

This product is a by-product collected by the dust collection system during the production of fused desilication zirconium in our company, containing a small amount of zirconia.

Telephone:

Key words:

Silica fume

Classification:

  • Product Description
  • Chemical Composition (%)

    Name

    Code

    Chemical Composition (%)

    SiO2

    Al2O3

    Fe2O3

    TiO2

    ZrO2

    Primary Powder

    SH-A

    >95

    <0.4

    <0.4

    <0.04

    2-5

    Secondary Powder

    SH-B

    >94

    <0.4

    <0.6

    <0.04

    2-5

    Tertiary Powder

    SH-C

    >90

    <0.8

    <0.8

    <0.04

    2-5

    Physical Performance Parameters

    Loose Bulk Density

    pH Value

    0.2-0.25g/cm³

    2-5

    Main Applications

    Used for manufacturing nano insulation boards, refractory casting material additives, corundum product additives, etc.

     