undefined
+
  • undefined

Yttrium Oxide Spray Granulation Powder

The yttrium oxide powder is a spray granulated powder of high-purity yttrium oxide, containing binders and other additives, suitable for pressing and forming, with a low sintering temperature, good ceramic properties, high whiteness of the sintered ceramic body, and free of impurities.

Telephone:

Key words:

Yttrium Oxide Spray Granulation Powder

Classification:

  • Product Description
  • Chemical composition (%)

    Code

    Chemical composition (%)

    Y2O3

    SiO2

    Al2O3

    Fe2O3

    TiO2

    CaO

    MgO

    Na2O

    Y2O3-RTP

    ≥99

    ≤0.05

    ≤0.05

    ≤0.05

    ≤0.05

    ≤0.05

    ≤0.05

    ≤0.05

    Physical performance parameters

    Appearance

    Sintered density

    Sintering shrinkage

    Sintering temperature

    Spray granulation powder

    4.90 g/cm3

    19-21%

    1600℃

    Product particle size

    Particle size (μm)

     -60+200

    Main applications

    Suitable for isostatic pressing and sintering of high-purity yttrium oxide ceramics.

     


Previous Magnesia zirconia powder

Next Yttrium Aluminum Garnet Spray Granulation Powder


Product inquiry

We will contact you within one working day. Please pay attention to your email.

All
  • All
  • Product Management
  • News