Fused yttrium oxide
Key words:
Fused yttrium oxide
Classification:
- Product Description
-
Chemical composition (%)
Code
Chemical composition (%)
Y2O3
Y2O3+ ∑R O
SiO2
Al2O3
Fe2O3
TiO2
DY-59
≥99.5
≤0.05
≤0.02
—
≤0.02
≤0.02
DY-60
≥99.5
≤0.05
≤0.02
—
≤0.02
≤0.02
Physical performance parameters
Code
DY-59
DY-60
Physical properties
Melting point 2410℃, true density 5.05g/cm³
Melting point 2415℃, true density 5.08g/cm³
Main applications
Can be used in the titanium casting industry and special ceramics industry, and can also be used as thermal barrier coating materials for graphite plates and others.
Previous Yttrium Aluminum Garnet Spray Granulation Powder
Next Silicon Zirconium Powder / High-Temperature Additive
Related Products
Product inquiry
We will contact you within one working day. Please pay attention to your email.
Contact Phone:
Focus on us

Online message
We will contact you within one working day. Please pay attention to your email.