Chemical Composition (%)
Name
Code
Chemical Composition (%)
ZrO2
Y2O3
SiO2
Al2O3
Fe2O3
TiO2
CaO
Gd2O3
Yb2O3
Yttrium-stabilized Zirconia
5PYD-b
>93
4.8-5.5
<0.4
≤0.2
≤0.1
≤0.2
≤0.2
-
-
7PYD-a
≥90
7.0-8.0
≤0.2
≤0.1
≤0.1
≤0.1
≤0.2
-
-
7PYD-b
≥90
7.0-8.0
≤0.2
≤0.2
≤0.1
≤0.2
≤0.2
-
-
7PYD-T
≥90
6.0-8.0
≤0.4
≤0.3
≤0.15
≤0.2
≤0.6
-
-
7PYD-aQ
≥90
7.0-8.0
≤0.1
≤0.1
≤0.1
≤0.1
≤0.1
-
-
7PYD-cQ
≥90
7.0-8.0
≤0.3
≤0.1
≤0.1
≤0.1
≤0.2
-
-
9PYD-b
≥88
8.8-9.8
≤0.4
<0.2
≤0.1
≤0.2
≤0.2
-
-
13PYD-b
≥84
13-14
≤0.3
<0.2
≤0.1
≤0.2
≤0.2
-
-
16PYD-a
≥81
15-17
≤0.1
≤0.1
≤0.1
≤0.1
≤0.1
-
-
20PYD-a
78.87
20.87
0.06
0.02
0.04
0.01
-
-
-
48PYD-a
51.19
48.56
0.05
0.01
0.05
0.01
-
-
-
Ytterbium-stabilized Zirconia
12PYbD-a
87.42
0.01
0.01
0.03
0.01
-
-
12.50
Yttrium-Ytterbium-stabilized Zirconia
5YYbD-a
79.92
5
0.01
0.01
0.03
0.01
-
-
15.00
Yttrium-Ytterbium-Gadolinium-stabilized Zirconia
3YYbGD-a
87.91
3.5
0.01
0.01
0.03
0.01
-
4.0
4.5
9YYbGD-a
79.40
9.7
0.02
0.01
0.03
0.01
-
5.2
5.6
Physical Performance Parameters
Code
5PYD-b
7PYD-a
7PYD-b
7PYD-T
7PYD-aQ
7PYD-cQ
9PYD-b
13PYD-b
16PYD-a
Physical Properties
Stabilization rate >50%, true density >5.7g/cm³
Stabilization rate 75-85%, true density >5.8g/cm³
Stabilization rate 75-85%, true density >5.8g/cm³
Stabilization rate 70-90%, true density >5.8g/cm³
Stabilization rate >95%, true density >5.8g/cm³
Stabilization rate >95%, true density >5.8g/cm³
Stabilization rate >95%, true density >5.8g/cm³
Stabilization rate 100%, true density >5.8g/cm³
Stabilization rate 100%, true density >5.7g/cm³
Main Applications
Setter plate for electro-ceramic industry, metering nozzles, submerged nozzles, zirconia bubble products, high-quality zirconia kiln furniture, alumina toughening ceramic additives, induction furnace insulation layer filling materials; manufacturing titanium alloy casting coating materials, graphite plate coating materials, alumina plate coating materials, and other high-temperature coating materials for plasma spraying on metal surfaces, oxygen-permeable ceramic rings, etc.
Previous Fused magnesia stabilized zirconia
Related Products
Product inquiry
We will contact you within one working day. Please pay attention to your email.
Contact Phone:
Focus on us
Online message
We will contact you within one working day. Please pay attention to your email.