Fused monoclinic zirconia
Key words:
Fused monoclinic zirconia
Classification:
- Product Description
-
Chemical composition (%)
Code
Chemical composition (%)
ZrO2+HfO2
SiO2
Al2O3
Fe2O3
TiO2
Z-31
≥98.5
≤0.60
≤0.40
≤0.04
≤0.20
Z-61
≥98.5
≤0.60
≤0.40
≤0.04
≤0.20
Z-91
≥99
≤0.20
≤0.30
≤0.04
≤0.20
Z-99
≥99
≤0.15
≤0.10
≤0.04
<0.15
Physical performance parameters
Appearance
Melting point
Specific gravity
Yellow/beige
2700 degrees
5.85g/cm3
Product particle size
Code
Z-31
Z-61
Z-91
Z-99 Particle size (μm)
12
3
Customizable
Main applications
Tundish nozzle, zirconia sliding gate, powder metallurgy nozzle, casting zirconia crucible, ceramic foam filter, ceramic pigment, soft magnetic ferrite embedded sand, zirconia welding rod, automobile brake pad, abrasives and other fields.
Next High-performance monoclinic zirconia
Related Products
Product inquiry
We will contact you within one working day. Please pay attention to your email.
Contact Phone:
Focus on us

Online message
We will contact you within one working day. Please pay attention to your email.